Shock-Wave Sintering of the 70 vol.% Kh13M2–30 vol.% Cr3C2 Carbonized Steel in a Wide Temperature Range
Crossref DOI link: https://doi.org/10.1007/s11106-017-9835-2
Published Online: 2017-02-14
Published Print: 2017-01
Update policy: https://doi.org/10.1007/springer_crossmark_policy
Tolochin, A. I.
Laptev, A. V.
Yakovenko, R. V.
Maslyuk, V. A.