Good Thermal Stability, High Permittivity, Low Dielectric Loss and Chemical Compatibility with Silver Electrodes of Low-Fired BaTiO3–Bi(Cu0.75W0.25)O3 Ceramics
Crossref DOI link: https://doi.org/10.1007/s11664-016-4898-2
Published Online: 2016-09-02
Published Print: 2017-01
Update policy: https://doi.org/10.1007/springer_crossmark_policy
Chen, Xiuli
Ma, Dandan
Chen, Jie
Huang, Guisheng
Zhou, Huanfu
Funding for this research was provided by:
National Natural Science Foundation of China (11464009, 11364012)
License valid from 2016-09-02