Laser Additive Manufacturing of (Ti-6Al-4V)/10 wt.% Ag Composite Using Spherical Powders to Reduce Wear and Friction
Crossref DOI link: https://doi.org/10.1007/s11665-018-3743-6
Published Online: 2018-11-14
Published Print: 2019-01
Update policy: https://doi.org/10.1007/springer_crossmark_policy
Li, Xiaoxue
Yang, Kang
Lin, Haibo
Ma, Hongru
Han, Yukun
He, Qiang
Text and Data Mining valid from 2018-11-14
Article History
Received: 26 December 2017
Revised: 6 August 2018
First Online: 14 November 2018