Hydrogen Damage in Carbon Steel Tubing: An Investigation of Various Macro-Failure Morphologies Observed in Boiler Water Wall Tubes Manifesting as Hydrogen Damage Failure
Crossref DOI link: https://doi.org/10.1007/s11668-024-02084-5
Published Online: 2024-12-21
Published Print: 2025-02
Update policy: https://doi.org/10.1007/springer_crossmark_policy
Gokhale, Aditya
Mangam, Subhakar
Singh, Chetan
Jain, Jayant
Das, Anil Kumar
Varma, Anand D.
Text and Data Mining valid from 2024-12-21
Version of Record valid from 2024-12-21
Article History
Received: 7 November 2024
Revised: 27 November 2024
Accepted: 10 December 2024
First Online: 21 December 2024