Effects of Cooling Rate on the Microstructure and Tensile Properties of Wire-Arc Additive Manufactured Ti–6Al–4V Alloy
Crossref DOI link: https://doi.org/10.1007/s12540-019-00563-1
Published Online: 2020-01-30
Published Print: 2020-08
Update policy: https://doi.org/10.1007/springer_crossmark_policy
Yi, Hui-Jun
Kim, Jin-Woo
Kim, Young-Lak
Shin, Sangyong https://orcid.org/0000-0002-4166-9910
Text and Data Mining valid from 2020-01-30
Version of Record valid from 2020-01-30
Article History
Received: 1 October 2019
Accepted: 27 November 2019
First Online: 30 January 2020