Preparation of W–TiC alloys from core–shell structure powders synthesized by an improved wet chemical method
Crossref DOI link: https://doi.org/10.1007/s12598-018-1066-2
Published Online: 2018-06-07
Published Print: 2023-04
Update policy: https://doi.org/10.1007/springer_crossmark_policy
Lang, Shao-Ting
Yan, Qing-Zhi http://orcid.org/0000-0001-7449-9404
Sun, Ning-Bo
Zhang, Xiao-Xin
Funding for this research was provided by:
ITER-National Magnetic Confinement Fusion Program (2014 GB123000)
Text and Data Mining valid from 2018-06-07
Version of Record valid from 2018-06-07
Article History
Received: 17 January 2017
Revised: 28 March 2017
Accepted: 8 May 2018
First Online: 7 June 2018