Effect of Solution Treatment and Aging Temperature on α′ and Ti3Al(α2) Phase Formation and Mechanical Properties of Water-Quenched Ti–6Al–4V
Crossref DOI link: https://doi.org/10.1007/s13632-021-00818-7
Published Online: 2022-03-11
Published Print: 2022-02
Update policy: https://doi.org/10.1007/springer_crossmark_policy
Vahidshad, Yaser
Khodabakhshi, Amir Hossein
Text and Data Mining valid from 2022-02-01
Version of Record valid from 2022-02-01
Article History
Received: 11 July 2021
Revised: 29 November 2021
Accepted: 7 December 2021
First Online: 11 March 2022