Porous APS YSZ TBC Manufactured at High Powder Feed Rate (100 g/min) and Deposition Efficiency (70%): Microstructure, Bond Strength and Thermal Gradients
Crossref DOI link: https://doi.org/10.1007/s11666-021-01302-y
Published Online: 2022-01-04
Published Print: 2022-02
Update policy: https://doi.org/10.1007/springer_crossmark_policy
Lima, Rogerio S.
Text and Data Mining valid from 2022-01-04
Version of Record valid from 2022-01-04
Article History
Received: 6 September 2021
Revised: 26 October 2021
Accepted: 26 November 2021
First Online: 4 January 2022