Effect of Hydrogen Corrosion on the Brittle Fracture Resistance of an Oil Line Pipe 530 mm in Diameter Made of 12GSB Ferritic–Pearlitic Steel
Crossref DOI link: https://doi.org/10.1134/S0036029520040084
Published Online: 2020-05-07
Published Print: 2020-04
Update policy: https://doi.org/10.1007/springer_crossmark_policy
Goritskii, V. M.
Shneiderov, G. R.
Goritskii, O. V.
Text and Data Mining valid from 2020-04-01
Version of Record valid from 2020-04-01
Article History
Received: 22 March 2019
Revised: 18 April 2019
Accepted: 24 April 2019
First Online: 7 May 2020